MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel 161 Tool Steel, High Carbon H13
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Crucible 161 is a high carbon modification of H13, intended for applications requiring higher hardness, compressive strength, wear resistance, or tempering resistance (hot hardness), at slightly lower toughness. It may be used at tool temperatures up to about 1000 F, with brief exposures up to 1100 F.

Information provided by Crucible Industries

Key Words: AISI H13
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 197 - 229
Hardness, Rockwell C 32.5
@Tempering Temp. 649 °C
air cooled from 1900°F then tempered
 44.5
@Tempering Temp. 621 °C
air cooled from 1900°F then tempered
 48.5
@Tempering Temp. 593 °C
air cooled from 1900°F then tempered
 52.5
@Tempering Temp. 566 °C
air cooled from 1900°F then tempered
 56.5
@Tempering Temp. 538 °C
air cooled from 1900°F then tempered
Modulus of Elasticity 30000 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.40 µin/in-°F
@Temperature 21.1 - 204 °C
 6.80 µin/in-°F
@Temperature 21.1 - 427 °C
 7.30 µin/in-°F
@Temperature 21.1 - 649 °C
Thermal Conductivity 174 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.50 %
Chromium, Cr 5.0 %
Iron, Fe 90.4 %as balance
Manganese, Mn 0.40 %
Molybdenum, Mo 1.6 %
Silicon, Si 1.0 %
Vanadium, V 1.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
AISI Type H13 Hot Work Tool Steel
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 450°C
Sandvik Osprey H13 Tool Steel Powder (Grade 80% - 22)

NCRUC938 / 160389

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.