Description: AFLAS® 200P (SPL-FKM) is a peroxide-curable specialty fluoroelastomer offering improved performance over conventional FKM-type fluoroelastomers in demanding applications found in the oil & gas, chemical process, industrial equipment, food handling, pharmaceutical, heavy duty diesel and automotive industries. AFLAS® 200P displays outstanding resistance to heat, acids & bases, many solvents, and ozone. Classified by ASTM D 1418-01 as TYPE IV FKM Material Features: Improved cold temperature performance (Tg = -13°C, TR-10 = -8°C) - Retains good base resistance and heat tolerance
- Can be solvated and applied as a coating
End User Benefits: Longer life of seals - Resists aggressive oils which contain anti-oxidants
- Improved sealing for cold application environments
Typical Applications: Oil seals - Shaft seals
- O-Rings
- Gaskets
Information provided by AGC Chemicals Americas Inc. |