MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Michelman® Release Coat® P1 Uncatalyzed portion of a two-part silicone release coating
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Uncatalyzed portion of a two-part silicone release coating

Usage: Release Coat® P1 is one part of a two part silicone release coating. A catalyzed release coat system offers superior release and in most cases FDA compliance. This system is not gluable.

Application Data: Release Coat® P1 must be combined with Catalyst P1 before applying to a substrate. This product may be applied by rod or blade coater.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.00 g/cc0.980 - 1.00 g/cc
pH 3.0 - 6.03.0 - 6.0
Brookfield Viscosity 300 - 800 cP300 - 800 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceWhite, semi-viscous liquid
Solids TypeSilicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHEL184 / 135101

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.