Zylar® 670 is an impact modified styrene acrylic copolymer that provides practical toughness, excellent clarity and superior processing characteristics for demanding injection molded applications. Excellent clarity, Exceptional performance in drop tests, Low density, Ease of processing, Low moisture absorption, Gamma & ETO sterilizableInformation provided by Styrolution. |