MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay EF1812 Polycarbosilane Polymer, Pyrolized with T300 Carbon Fabric
Categories: Ceramic; Carbide

Material Notes: EF1812 is a polycarbosilane polymer prepreg system specially formulated for the manufacture of ceramic matrix carbon fiber reinforced components operating at high temperature. After laminating and curing in a conventional manner, the component requires a six-stage Polymer Infiltration and Pyrolysis (PIP) cycle. This process converts the polycarbosilane into a silicon carbide-silicon oxycarbide (SiC-SiOC) matrix. Typical applications include lightweight heat shields and ducts which are subject to elevations in temperatures of up to 800°C (1472°F) for short periods of time. The life expectancy of components made from EF1812 depends on the time, temperature and nature of the hot environment, and must be determined by in-situ tested.

Features & Benefits:

  • 5 day tack life at 21°C (70°F) with both release films in position
  • 12 months storage at -18°C (0°F)
  • Autoclave processing
  • EF1812 is supplied on T300 woven carbon fiber as standard
  • Typical cure 6 hrs at 190°C (356°F)
  • Suitable for high temperature applications
  • Requires 6 stage Polymer Infiltration and Pyrolysis (PIP) cycle to fully densify
  • EF1812 is suitable for light-load bearing applications
Mechanical property data for EF1812-heat treated T300 plain weave carbon fabric 200g/cm2; Cure: 6 hrs at 190° (374°F), 6.2 bar (90 psi), followed by 6 PIP cycles. Tested dry at room temperature.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/cccured laminate
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 22680 psi0/90° Orientation; LIS/MEC/059
Tensile Modulus 26.4 GPa0/90° Orientation; LIS/MEC/059
Flexural Strength 275400 psi0/90° Orientation; LIS/MEC/250
 314000 psi0/90° Orientation, Exposure: 1 hr at 400°C; LIS/MEC/250
 329000 psi0/90° Orientation, Exposure: 1 hr at 600°C; LIS/MEC/250
Flexural Modulus 50.2 GPa0/90° Orientation; LIS/MEC/250
 60.3 GPa0/90° Orientation, Exposure: 1 hr at 600°C; LIS/MEC/250
 61.4 GPa0/90° Orientation, Exposure: 1 hr at 400°C; LIS/MEC/250
Shear Strength 3770 psi0/90° Orientation Interlaminar; LIS/MEC/252
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 800 °Cshort term
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 hour
@Temperature 190 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Solvay CYCOM® 977-6 Epoxy Prepreg Laminate with T300 Plain Weave Fabric

PCYTED170 / 180472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.