Description: Technipol® 180 D is a co-polyester based thermoplastic adhesive designed for the production of air and oil filters in the automotive industry. Technipol® 180 D is characterized by: - a high chemical resistance (mineral oil and diesel vapors)
- a high thermal resistance, compatible with paper curing temperatures
- a high elasticity, that assures the integrity of the filter during all production steps
Information provided by SIPOL SpA |