MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Murdopol® Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its ability to create firm plastic/metal connections.

Special Properties:
• Good shock and impact resistance
• Low residual stress
• Metal core surrounded by cast plastic available
• Good damping and vibration behavior
• Lowest moisture absorption of all polyamides
• Good resistance to chemicals
• Dimensionally stable

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PA 12-G
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.90 %
@Temperature 23.0 °C
50% RH
Water Absorption at Saturation 1.4 %
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78DIN 53505
Tensile Strength, Yield 55.0 MPadry; ISO 527-1
 55.0 MPa50% RH; ISO 527-1
Elongation at Break 200 %dry; ISO 527-1
 200 %50% RH; ISO 527-1
Modulus of Elasticity 2.00 GPadry
 2.00 GPa50% RH
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 20.0 kJ/m²dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35
Sand Slurry 0.80µm/km
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cm50% RH; IEC 60093
 >= 1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance >= 1.00e+12 ohm50% RH; IEC 60093
 >= 1.00e+13 ohmdry; IEC 60093
Dielectric Constant 3.5
@Frequency 100 Hz
dry; IEC 60250
Dielectric Strength 20.0 kV/mm50% RH; IEC 60243-1
 50.0 kV/mmdry; IEC 60243-1
Dielectric Loss Index 0.038
@Frequency 100 Hz
dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
 120 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.230 W/m-K
Melting Point 180 °CISO 11357-1
Maximum Service Temperature, Air 120 °C
@Time 1.80e+7 sec
 150 °C
@Time <=86400 sec
Minimum Service Temperature, Air -60.0 °C
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CENTROPLAST CENTROMID 12 Polyamide 12
BASF Elastollan® 1154 D KFFC TPUR
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive

PMURT925 / 156572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.