MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Beta Processed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Information provided by Allvac and the references. Alpha-Beta Alloy. Beta Transus 890ºC. Solution Treated 800ºC, 4h; Aged 635ºC, 8h.

Applications: Compressor discs, heavy section forgings for gas turbine engine components.

Characteristics: High tensile strength, good crack growth/fatigue resistance and good fracture toughness.

Forms typically available: Billet and bar.

1 other heat treatment of this alloy is in MatWeb.

Key Words: UNS R58650
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 369Estimated from Rockwell C.
Hardness, Knoop 403Estimated from Rockwell C.
Hardness, Rockwell C 40
Hardness, Vickers 386Estimated from Rockwell C.
Tensile Strength, Ultimate 1180 MPa
Tensile Strength, Yield 1050 MPa
Elongation at Break 11 %
Modulus of Elasticity 115 GPaalpha-beta processed
Notched Tensile Strength 1350 MPaKt (stress concentration factor) = 4.0
Poissons Ratio 0.33Typical for alpha-beta titanium alloy.
Fracture Toughness 53.0 MPa-m½K(IC)
Shear Modulus 43.2 GPaCalculated from typical values.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000160 ohm-cmEstimated from similar alpha-beta titanium alloys.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
@Temperature 20.0 - 100 °C
Typical alpha-beta titanium alloy
 9.70 µm/m-°C
@Temperature 20.0 - 400 °C
Specific Heat Capacity 0.525 J/g-°CTypical value for titanium alloys.
Thermal Conductivity 7.80 W/m-K
Beta Transus 890 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.0 %
Chromium, Cr 4.0 %
Hydrogen, H <= 0.0125 %
Iron, Fe <= 0.30 %
Molybdenum, Mo 4.0 %
Nitrogen, N <= 0.040 %
Oxygen, O 0.080 - 0.13 %
Tin, Sn 2.0 %
Titanium, Ti 83 %
Zirconium, Zr 2.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Alpha-Beta Processed
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age
Alclad Aluminum 7075-T6, T651
Titanium Ti-6Al-4V (Grade 5), STA Bar
Titanium Ti-6Al-4V (Grade 5), STA

MTP172 / 14228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.