MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Synfoam® SW-18 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Pre-cast. SynFoam SW is a pressure resistant syntactic foam designed to provide buoyancy for underwater depths up 1,000 meters. SW is a closed cell foam that is easy to machine and will provide a smooth surface after sanding. SynFoam SW is ideal for underwater robotics, vehicles, flotation, pumps and as a core material. SynFoam SW resists water absorption and provides excellent performance for in shallow subsea applications. It has been used as a replacement for PU and PVC based foams due to its higher strength, better chemical resistance, and UV stability. SynFoam SW is available as 6” x 12” x 24” fully cured blocks. The blocks may be further machined into different sizes and shapes by the end user to meet the necessary specific tolerances and requirements. Our syntactic foam is easily bonded together with the use of our syntactic adhesive to form large structures.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.256 - 0.320 g/cc0.00926 - 0.0116 lb/in³
Moisture Absorption <= 5.00 %<= 5.00 %24 hours @ depth
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 6.41 MPa930 psi
 
Descriptive Properties
Depth Rating (m)500
Service Pressure (psi)735

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNF025 / 192900

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.