MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici RADILON® A RV300RKC2 306 BK Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: PA66 30% glass fiber reinforced injection molding grade. Improved resistance to disinfectants. Heat stabilized. Drinking water and food contact. Black color. Product with good resistance to hydrolysis and improved resistance to disinfectants, specifically intended for use in applications in civil and industrial water management as well as appliances, requiring high stiffness and good mechanical resistance.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, Food Contact, Drinking Water Contact, UL Listed

Industries: Consumer Industry Goods, Water Management

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 6.2 %
@Thickness 2.00 mm
Immersion at 23°C; ISO 62
Moisture Absorption 1.60 %
@Thickness 2.00 mm
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 300/90/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cmMelt Temp/Mold Temp/Cavity Pressure: 300/90/60; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 175 MPa5mm/min; ISO 527-2/1A
Elongation at Break 3.2 %5mm/min; ISO 527-2/1A
Tensile Modulus 9800 MPa1mm/min; ISO 527-2/1A
Flexural Strength 270 MPa2mm/min; ISO 178
Flexural Modulus 9200 MPa2mm/min; ISO 178
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 78.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm500V; IEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75/2Af
Vicat Softening Point 255 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADICI077 / 313578

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.