Petropol Tenogel® A3 HF NTLA010 AB308 ABS
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Product Description: High Flow, ABS
Resin ID (ISO 1043): ABS
Additive: High Flow
Processing: Injection Molding; Extrusion
Color: Natural
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.04
g/cc
0.0376
lb/in³
ASTM D792/A
Melt Flow
37
g/10 min
@Load 10.0 kg,
Temperature 220 °C
37
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238/A
Mechanical Properties
Metric
English
Comments
Tensile Strength
45.0
MPa
6530
psi
ASTM D638
Flexural Strength
65.0
MPa
9430
psi
ASTM D790
Flexural Modulus
2.45
GPa
355
ksi
ASTM D790
Izod Impact, Notched
2.40
J/cm
4.50
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
96.0
°C
205
°F
ASTM D648
Vicat Softening Point
102
°C
216
°F
ISO 306/A50
Flammability, UL94
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Processing Properties
Metric
English
Comments
Processing Temperature
200
-
240
°C
392
-
464
°F
Molding
Mold Temperature
60.0
-
80.0
°C
140
-
176
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
4.00
hour
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PPETROPOL350 / 313258
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.