MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Technoprene® A60K4 Glass-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Standard Technoprene® 20% Glass-Reinforced Polypropylene

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Water Absorption 0.020 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0070 cm/cmSO.F.TER Method
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength 75.0 MPaASTM D638
Flexural Strength 115 MPaASTM D790
Flexural Modulus 4300 MPaASTM D790
Izod Impact, Notched 90.0 J/m
@Temperature -20.0 °C
ASTM D256/A
 115 J/m
@Temperature 23.0 °C
ASTM D256/A
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 2.4ASTM D150
Comparative Tracking Index >= 650 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 70.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 145 °CASTM D648
Vicat Softening Point 128 °C50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
RTP Company RTP 102 CC HF  Polypropylene (PP) Glass Fiber 15% - Chemically Coupled - High Flow
Röhm Plexiglas® 8N PMMA Molding Compound
Oxford Polymers Stranox C-PP15% Glass Fiber Reinforced Polypropylene, Lightweight

PSOFS811 / 162275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.