MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) PVC-S6058 Poly Vinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Grade S6058 has low porosity & very high bulk density. Therefore it is most suitable for rigid applications, high machine throughput, and specific applications as additive polymer.

Applications: extrusion of flexible sections and hoses, calendaring.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.580 g/ccDIN-53466
Volatiles <= 0.20 %weight %; ISO R-1269
Viscosity Test 88 cm³/gDIN-53726
Ash <= 0.050 %Sulfate ash, weight %; DIN-53568/2
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 56 %by weight
 
Descriptive Properties
Dark Resin, particles30per 250 g PVC; HULS-6.9
K-Value60DIN-53726
Residual Vinyl Chloride Monomer, ppm=1HULS-6.11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) PC 1218 Polycarbonate
Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber
Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride
Iran Petrochemical (PCC) PC 1822 Polycarbonate

PIPC324 / 149758

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.