MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their performance under specific conditions. The manufacturing process for each grade is tightly controlled to produce materials that have a uniform microstructure and the right balance of strength, grain size and hardness to offer optimum performance for their intended applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 3.12 g/cc0.113 lb/in³
Particle Size 5.0 µm5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength, Yield 65.0 MPa9430 psiEstimated at 70% of flexural strength
Flexural Strength 117 MPa17000 psi
Compressive Strength 210 MPa30500 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000270 ohm-cm0.000270 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.50 µm/m-°C4.72 µin/in-°F
Thermal Conductivity 175 W/m-K1210 BTU-in/hr-ft²-°F
 
Descriptive Properties
Oxidation Threshold500°C1% weight loss in 24 hours. Increases by approximately 100°C if graphite is purified.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite ACF-10Q Industrial Grade Graphite
Poco Graphite ZXF-5Q Industrial Grade Graphite
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite
Poco Graphite AXZ-5Q Industrial Grade Graphite
UCAR Carbon UCAR® PGW Pressure Molded Graphite

CPOCO16 / 85593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.