MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DIAB Divinycell® H 250 Sandwich Core Material
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: Divinycell H has been widely used over many years in virtually every application area where sandwich composites are employed including the marine (leisure, military and commercial), land transportation, wind energy, civil engineering/infrastructure and general industrial markets. In its application range, Divinycell H has the highest strength to density ratio. It exhibits at both ambient and elevated temperatures impressive compressive strength and shear properties. In addition the ductile qualities of Divinycell H make it ideal for applications subject to fatigue, slamming or impact loads.

Other key features of Divinycell H include consistent high quality, excellent adhesion/peel strength, excellent chemical resistance, low water absorption and good thermal/acoustic insulation. Divinycell H is compatible with virtually all commonly used resin systems (polyester, vinyl ester and epoxy) including those with high styrene contents. Its good temperature performance with high residual strength and good dimensional stability makes Divinycell H ideal for hand laminating, vacuum bagging, RTM (resin transfer molding) or vacuum infusion.

Continuous operating temperature is -200 to 70°C. The foam can be used in sandwich structures, for outdoor exposure, with external skin temperatures up to 85°C. Normally Divinycell H can be processed up to 90°C with minor dimensional changes. Maximum processing temperature is dependent on time, pressure and process conditions.

Information Provided by DIAB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.250 g/ccISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 9.20 MPaPerpendicular to the plane; ASTM D1623
Elongation at Break 40 %In Shear; ASTM C273
Tensile Modulus 320 MPaPerpendicular to the plane; ASTM D1623
Compressive Strength 6.20 MPaPerpendicular to the plane; ASTM D1621
Compressive Modulus 300 MPaPerpendicular to the plane; ASTM D1621
Shear Modulus 0.104 GPaASTM C273
Shear Strength 4.50 MPaASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.2 µin/in-°F
Maximum Service Temperature, Air 70.0 °CContinuous
Minimum Service Temperature, Air -200 °CContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB Divinycell® H 130 Sandwich Core Material
DIAB Divinycell® H 100 Sandwich Core Material
DIAB Divinycell® F 90 Sandwich Core Material
DIAB Divinycell® H 60 Sandwich Core Material
DIAB Divinycell® H 80 Sandwich Core Material

PDIAA927 / 99165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.