Zylar® 765 is a MBS grade that provides very high toughness, good clarity and superior processing characteristics for demanding injection molding applications. High clarity, High toughness, Low density, Gamma & ETO sterilizable. Applications: Appliance and consumer goods, Office accessories, Industrial housings and covers, Displays, ToysInformation provided by Styrolution. |