MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.

Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but with significantly higher stiffness (elastic modulus). Due to the use of iron as the beta stabilizer, the alloy has lower formulation costs than TIMETAL 6-4. The combination of reasonable cost and excellent mechanical properties make TIMETAL 62S a practical substitute for many engineering materials.

Typical heat treatment for this alloy: Mill Anneal at 760°C for 1-2 hrs, air cool

Data provided by TIMET.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.44 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 986 MPaTypical Longitudinal
 1014 MPaTypical Transverse
Tensile Strength, Yield 945 MPa
@Strain 0.2 %
Longitudinal, typical
 972 MPa
@Strain 0.2 %
Transverse, typical
Elongation at Break 16 %Typical Transverse in 2 in (50 mm)
 18 %Typical Longitudinal in 2 in (50 mm)
Reduction of Area 30 %Transverse
 37 %Longitudinal
Modulus of Elasticity 128 GPaTypical
Fracture Toughness 48.0 MPa-m½K(IC); L-T Orientation
 52.0 MPa-m½K(IC); T-L Orientation
Bend Radius, Minimum 4.5 t
@Thickness 2.00 mm
Typical; sheet
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000163 ohm-cm
 0.000169 ohm-cm
@Temperature 127 °C
 0.000180 ohm-cm
@Temperature 327 °C
 0.0001845 ohm-cm
@Temperature 727 °C
 0.000185 ohm-cm
@Temperature 540 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.60 µm/m-°C
@Temperature 20.0 °C
 9.70 µm/m-°C
@Temperature 250 °C
 10.6 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 0.500 J/g-°C
 0.160 BTU/lb-°F
@Temperature 427 °C
Beta Rolled plus Recrystallization Annealed
 0.170 BTU/lb-°F
@Temperature 760 °C
Beta Rolled plus Recrystallization Annealed
Thermal Conductivity 8.60 W/m-K
 88.0 BTU-in/hr-ft²-°F
@Temperature 427 °C
Beta Rolled plus Recrystallization Annealed
 115 BTU-in/hr-ft²-°F
@Temperature 760 °C
Beta Rolled plus Recrystallization Annealed
Beta Transus 1024 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.0125 %
Iron, Fe 1.3 - 2.0 %
Nitrogen, N <= 0.040 %
Other, total <= 0.30 %
Oxygen, O 0.15 - 0.20 %
Silicon, Si 0.070 - 0.13 %
Titanium, Ti 90.7 - 93 %Calculated as remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); ST 1550°F (843°C) + Aged at 538°C
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Rolled plus Mill Annealed

NTIME62SB / 19318

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.