MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Duomeen O Oleyl propylene diamine
Categories: Other Engineering Material

Material Notes: Duomeen O is an oleylpropylene diamine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.810 g/cc
@Temperature 70.0 °C
0.0293 lb/in³
@Temperature 158 °F
 0.817 g/cc
@Temperature 60.0 °C
0.0295 lb/in³
@Temperature 140 °F
 0.831 g/cc
@Temperature 40.0 °C
0.0300 lb/in³
@Temperature 104 °F
 0.841 g/cc
@Temperature 25.0 °C
0.0304 lb/in³
@Temperature 77.0 °F
Viscosity  14 cP
@Temperature 35.0 °C
14 cP
@Temperature 95.0 °F
 17 cP
@Temperature 30.0 °C
17 cP
@Temperature 86.0 °F
 19 cP
@Temperature 25.0 °C
19 cP
@Temperature 77.0 °F
Vapor Pressure  0.000300 bar
@Temperature 18.0 °C
0.225 torr
@Temperature 64.4 °F
 0.00100 bar
@Temperature 43.0 °C
0.750 torr
@Temperature 109 °F
 0.00220 bar
@Temperature 65.0 °C
1.65 torr
@Temperature 149 °F
 0.00520 bar
@Temperature 93.0 °C
3.90 torr
@Temperature 199 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.54 J/g-°C
@Temperature 37.8 °C
0.606 BTU/lb-°F
@Temperature 100 °F
 2.58 J/g-°C
@Temperature 60.0 °C
0.617 BTU/lb-°F
@Temperature 140 °F
 2.61 J/g-°C
@Temperature 71.1 °C
0.623 BTU/lb-°F
@Temperature 160 °F
 2.68 J/g-°C
@Temperature 82.2 °C
0.641 BTU/lb-°F
@Temperature 180 °F
Melting Point 12.0 °C53.6 °F
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
>= 572 °F
@Pressure 14.6921 psi
Pour Point 18.0 °C64.4 °F
Flash Point >= 149 °C>= 300 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 5.00.00 - 5.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %
 
Descriptive Properties
Amine number320-350 mg KOH/g
AppearanceLiquid
Cloud point29°C
Content= 43 %Primary Amine
 = 43 %Secondary Amine
 = 60 g I2/100 gIodine value
 = 90 %Apparent diamine activity
Equivalent mass163 g/eq
HLB15Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY493 / 286016

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.