MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toho Tenax Besfight® G30-500 6K HTA-7C EP03 Continuous Filament Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiber
Typical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/cc
Fiber Count 4050 dtex
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 640000 psi
Elongation at Break 1.9 %
Tensile Modulus 3.40e+7 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00150 ohm-cm
 
Descriptive Properties
Filament Diameter7 µm
Size Level1.3%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toho Tenax Besfight® G30-700 24K HTA-7D F402 Continuous Filament Carbon Fiber
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Glassy Carbon used in heart valve prostheses
Graphite, Carbon, C

ETOHO24 / 6114

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.