MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Butyl Acrylate
Categories: Fluid

Material Notes: Formula: C7H12O2

CAS: 141-32-2

Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.

Applications: Butyl acrylate forms homopolymers and copolymers. Copolymers of butyl acrylate can be prepared with acrylic acid and its salts, amides and esters, and with methacrylates, acrylonitrile, maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils, etc. Butyl acrylate is also a very useful feedstock for chemical syntheses, because it readily undergoes addition reactions with a wide variety of organic and inorganic compound.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.898 g/cc
Viscosity Measurement 0.92[mPa.s}
Molecular Weight 128.2 g/mol
Vapor Pressure 0.00540 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.93 J/g-°Cof liquid
Melting Point -64.0 °CFreezing Point
Boiling Point 148 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4185
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM E203
 
Descriptive Properties
Acidity, as HCI0.01as acrylic acid, ASTM D1613
Assay>99.5%
Color<10APHA, ASTM D1209
Heat of Polymerization504 kJ/kg
Latent Heat of Evaporation at Boiling Point292 kJ/kg
Standard Stabilization10 - 20 ppmMEHQ, ASTM D3125

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Glacial Acrylic Acid
BASF 2-Ethylhexanol
BASF N-Butanol
Avient Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Avient Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)

PBASG0891 / 132524

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.