Product Description: R08G-01 is a random copolymer polypropylene for film, blow molding, expanded PP foam beads, and injection molding applications with a barefoot additive package. Availability: North America Additive: Slip Features: Food Contact Acceptable; Random Copolymer; Slip Uses: Blow Molding Applications; Film; Foam Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520 RoHS Compliance: Contact Manufacture Forms: Pellets Processing Method: Blow Molding; Film Extrusion; Foam Processing; Injection MoldingInformation provided by INEOS Olefins & Polymers USA |