MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating
Categories: Fluid

Material Notes: LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozone and fluid resistance on a wide variety of substrates while having very low VOCs.

HPC-6B is black; HPC-6C is clear and colorable. Coatings are composed of a mixture of polymers, organic compounds and fillers dissolved or dispersed in an organic solvent system. Additionally, the HPC-6C coating mixes well with colored pigments allowing for the creation of colored coatings.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/cc
Solids Content 10.9 %by weight
 13.6 %by volume
Brookfield Viscosity 50 - 300 cP
@Temperature 25.0 °C
LVT, Spindle #2 @ 30rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 20.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 121 °C
Let sit for 24 hours to develop a final cure
 >= 24.0 hour
@Temperature 25.0 °C
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
 
Descriptive Properties
AppearanceBlack
ConsistencyLiquid
SolventsPCBTF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Optiflo® T1000 (Formerly RXL-7301) Polymer
Bostik Tube & Tile Caulk Siliconized-Acrylic Caulk
Blue River Coatings Acrylic 4000 Topcoat
Saint-Gobain Normount® V2800 Energy-Dissipating High-Performance Polyurethane Foam with Acrylic Adhesive
Mallard Creek Polymers Rovene® 6087 Styrene-Acrylic Emulsion

PLORD144 / 86152

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.