MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hanwha Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applications. Typically used in non-structural applications where a very high strength to weight ratio is required, such as:

  • Automotive headliners
  • Door panels
  • Package shelves
  • Other interior trim

Physical properties apply only to bare SuperLite sheet and do not include surface films or scrim. Mechanical properties measured on flat plaques.

Draw ratio is defined as the ratio of the maximum depth of the mold to the minimum distance across the open face of the mold at any given location and is measured on flat plaques.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.370 g/ccASTM D3574
Filler Content 55 %ASTM D5630
Thickness 4000 - 4500 micronsTypical free lofted thickness after heating
Linear Mold Shrinkage <= 0.00020 cm/cmTypical, molds cut to zero
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPaASTM D638
Tensile Modulus 2.27 GPaASTM D638
Flexural Strength 7.00 MPaSAE J949
Flexural Modulus 1.42 GPaSAE J949
Impact 500N Multi-axial, 23°C, at max. load, measured on flat plaques; ASTM D3763
Impact Test 4.00 J
@Temperature 23.0 °C
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Instrumented Impact Energy at Peak 2.00 J
@Temperature 23.0 °C
Multi-axial, at max. load; ASTM D3763
 
Descriptive Properties
Available ColorsNatural and Charcoal
Draw RatioMax 1.5:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hanwha Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
Hanwha Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
Hanwha Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
Hanwha Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
Hanwha Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)

PZZGEAZ02 / 40551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.