MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aperam Superimphy® 286 Bar-Corrosion application
Categories: Metal; Ferrous Metal

Material Notes: An alloy Fe, Ni, Cr, Mo and Ti that is precipitation hardenable for high mechanical properties (notably for creep resistance). It presents a good strength and oxidation resistance at elevated temperature up to 700°C. It is a non- magnetic alloy.

Applications:

  • Energy (Turbine components)
  • Oil and gas industries
  • Aeronautic (compressors parts, bolts)
Standards related to these applications : ASTM A638, A453; AMS 5726, 5731, 5732, 5734, 5737, 5895

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 13.5 - 16 %
Iron, Fe 53.15 - 59.6 %
Molybdenum, Mo 1.0 - 1.5 %
Nickel, Ni 24 - 27 %
Titanium, Ti 1.9 - 2.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy (UNS S66286)
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age

NPERA021 / 194810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.