Characteristics: Promyde B36 L is a high viscosity polyamide 6 lubricated for injection and extrusion. Applications: Promyde B36 L allows a fast and efficient mould filling and an easy mould release, that combined with its excellent mechanical and thermal properties, make it suitable for components used in technical parts in mechanical, automotive, electrical and electronic industries. Information provided by Nurel Engineering Polymers |