MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® A-60-F Food Process Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process Tubing will outlast and outperform virtually all other food grade tubings. Even following extended exposure to heat and ozone, Norprene® Food Process Tubing will not crack or deteriorate as commonly found when using traditional rubber tubings. Extremely flexible, Norprene® Food Process Tubing resists kinks and retains its shape while installing quickly and easily. Its excellent flexural fatigue resistance makes it the absolute best choice for use in peristaltic pumps often found in dispensing equipment. Repeatedly autoclavable, Norprene® Food Process Tubing can be steam cleaned in place, eliminating the need for frequent tubing replacement. When harsh sanitizing solutions are used, it exhibits exceptional chemical resistance and is entirely unaffected by a wide variety of cleaning solutions. Also available with reinforcement to withstand elevated working pressure.

Features/Benefits:
  • Long flex life in peristaltic pumps
  • Temperature resistant from -60°F to 275°F
  • Compatible with virtually all common sanitizers and cleaners
  • Ozone and UV light resistant
  • Repeatedly autoclavable
  • Chemically compatible with a wide range of fluids
  • Meets FDA, 3-A and NSF criteria
Typical applications include Cosmetic Production, Food and Dairy Processing, Hot Beverage Dispensing, Water Purification Lines, Sanitizer Delivery, Soap Dispensing, Pesticide/Fertilizer Delivery, Ink and Toner Feed Lines, Chemical Transfer.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D792-91
Water Absorption 0.30 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6115 seconds; ASTM D2240-97
Tensile Strength, Yield 1000 psiASTM D412-97
Elongation at Break 375 %ASTM D412-97
100% Modulus 0.410 ksi
@Strain 100 %
ASTM D412-97
300% Modulus 0.800 ksi
@Strain 300 %
ASTM D412-97
Tear Strength 120 pliInitial Tear Strength; ASTM D1004-93
Compression Set 27 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 47 %at 75% Elongation; ASTM D412-97
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 535 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 275 °F
Brittleness Temperature -75.0 °FASTM D746-95
 
Descriptive Properties
ColorCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems

PSTGQZ199 / 68713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.