MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymax® Maxelast® D6770 TPE, Extruded
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade

Material Notes: Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.
    Uses:
  • Consumer Products
  • Toys & Novelties
  • Auto Parts
  • Sporting Goods
  • Seals
  • Wire & Cable Electronics
  • Medical Devices

Information from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 10.0 sec
ASTM D2240
Tensile Strength, Yield 1030 psiASTM D412
Elongation at Break 490 %ASTM D412
100% Modulus 0.413 ksi
@Strain 100 %
ASTM D412
300% Modulus 0.715 ksi
@Strain 300 %
ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Ethylene Propylene Rubber (EPM, EPDM)
Avient Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Polymax® Maxelast® D6760 TPE, Extruded
Polymax® Maxelast® D6890 TPE, Extruded

PMAXEL068 / 121155

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.