System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Taro Plast Taroblend 65 X0 PC/ABS, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
PC/ABS alloy, medium thermal resistance, low halogen content flame retardant UL94 V0, without antimony trioxide. Available: all colors, UV stabilized (L).
Information provided by Taro Plast S.p.a.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.18
-
1.20
g/cc
0.0426
-
0.0434
lb/in³
ISO 1183
Water Absorption
0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ISO 62
Water Absorption at Saturation
0.60 %
0.60 %
ISO 62
Linear Mold Shrinkage, Flow
0.0040
-
0.0070
cm/cm
0.0040
-
0.0070
in/in
ISO 2577
Linear Mold Shrinkage, Transverse
0.0040
-
0.0070
cm/cm
0.0040
-
0.0070
in/in
ISO 2577
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
50.0
MPa
7250
psi
ISO 527
Tensile Strength, Yield
65.0
MPa
9430
psi
ISO 527
Elongation at Break
45 %
45 %
ISO 527
Tensile Modulus
2.50
GPa
363
ksi
ISO 527
Flexural Strength
85.0
MPa
12300
psi
ISO 178
Flexural Modulus
2.45
GPa
355
ksi
ISO 178
Izod Impact, Notched
4.50
J/cm
8.43
ft-lb/in
127x12.7x3.2; ASTM D256
Charpy Impact Unnotched
NB
NB
80x10x4; ISO 179/1eU
Charpy Impact, Notched
2.00
J/cm²
9.52
ft-lb/in²
80x10x4; ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
ASTM D257
Comparative Tracking Index
200
V
200
V
Method A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
70.0
µm/m-°C
38.9
µin/in-°F
ISO 11359
Maximum Service Temperature, Air
60.0
°C
@Time 72000 sec
140
°F
@Time 20.0 hour
IEC 60216
Hot Ball Pressure Test
125
°C
257
°F
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi)
110
°C
230
°F
ISO 75/A
Vicat Softening Point
115
°C
@Load 5.00 kg
239
°F
@Load 11.0 lb
ISO 306
125
°C
@Load 1.00 kg
257
°F
@Load 2.20 lb
ISO 306
Flammability, UL94
V-0
@Thickness 1.70 mm
V-0
@Thickness 0.0669 in
127x2.17xThickness
Oxygen Index
32 %
32 %
6.3x12.7x3.2; ASTM D2863
Glow Wire Flammability Index
960
°C
@Thickness 2.00 mm
1760
°F
@Thickness 0.0787 in
60x60xThickness; IEC 60695-2-12
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PTARO107 / 283215
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.