MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys ImerPlast™ 10WPCT Recycled Polyolefin Resin
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyolefin

Material Notes: A black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. With added reinforcing filler and wood flour dispersant, ImerPlastTM 10WPCThas been shown to significantly improve extruder output. Melt filtered to 250 µm to ensure no particulates.

Information provided by Imerys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
 2.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 22.0 MPa
Tensile Modulus 1.60 GPa
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.05 %as packed
 
Descriptive Properties
ColorDark Gray
Melt Filtration250 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, Dry As Molded
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Concrete, expanded clay aggregate
Clay, Soft Shale
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade

PIMERY989 / 176006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.