MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo CoolPoly® D5522 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Product Description: CoolPoly D5522 offers thermal conductivity, excellent mechanical strength, surface appearance, low warpage, and excellent dimensional stability. Application of this grade is for a part with thin wall design in automotive and electronics. The D series is electrically non-conductive and can be used for its dielectric properties.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Low Warpage

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccISO 1183
Water Absorption 0.030 %Equilibrium, 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20700 psiISO 527-2/50
Elongation at Break 2.7 %ISO 527-2/50
Tensile Modulus 2.03e+6 psiISO 527-1
Flexural Strength 23200 psiISO 178
Flexural Modulus 1.89e+6 psiISO 178
Charpy Impact Unnotched 14.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.63
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 760 V/milIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 4.40 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 33.0 µin/in-°FISO 11359-2
Specific Heat Capacity 0.330 BTU/lb-°FASTM E1461
Thermal Conductivity 4.20 BTU-in/hr-ft²-°FThruplane; ASTM D1461
 6.90 BTU-in/hr-ft²-°FCrossflow; ASTM D1461
 17.0 BTU-in/hr-ft²-°FFlow; ASTM D1461
Melting Point 626 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 464 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 572 - 590 °F
Middle Barrel Temperature 590 - 608 °F
Front Barrel Temperature 608 - 626 °F
Nozzle Temperature 626 - 644 °F
Zone 4 626 - 644 °FInjection
Melt Temperature 626 - 653 °F
Mold Temperature 248 - 284 °F
Drying Temperature 302 °F
Dry Time 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6270 / 310963

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.