MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

MOL Group TATREN HG 10 07 PP, Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: TATREN HG 10 07 is a homopolymer of good processing stability and excellent spinning properties. It is characterized by broad processing window and it enables to process this grade by different processing technologies - fibers, cast film and injection molding. This grade contains anti gas fading additive package. It contains neither slip nor antiblocking agent.

Applications: TATREN HG 10 07 is intended especially for staple fibers production. It is also suitable for cast film production as core layer at co-extrusion and for injection molding of sanitary equipments, caps, closures and small technical items. This grade is partially suitable for sheet extrusion and thermoforming applications and for compounding.

(1) Typical properties measured on standard injection molded test specimen according to ISO 294-1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 1041041; ISO 2039-2
Tensile Strength, Yield 36.0 MPa5220 psi1; ISO 527-1,2
Elongation at Yield 8.0 %8.0 %1; ISO 527-1,2
Modulus of Elasticity 1.90 GPa276 ksi1, in Tension; ISO 527-1,2
Flexural Modulus 1.90 GPa276 ksi1; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²1; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °F1, flatwise; ISO 75-1,2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 260 °C410 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG078 / 297244

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.