MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Redwood Plastics REDCO™ PVM Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Redco™ PVM (pressure/velocity/maximum) was developed to provide a premium material for a variety of applications. Redco™ PVM is a self lubricated material with a low coefficient of friction that can increase the life of equipment. Redco™ PVM offers exceptional PV (pressure x velocity) values resulting in an excellent material for tough load bearing/frictional applications.

Typical Applications: Bearings, bushings, wear pads, sharp chain beds, gears, sprockets and power transmission components, and custom components.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Water Absorption 4.0 %4.0 %Equilibrium
 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.9 MPa
@Time 86400 sec
10000 psi
@Time 24.0 hour
Elongation at Break 20 %20 %
Tensile Modulus 2.96 GPa430 ksi
Flexural Strength 89.6 MPa13000 psi
Flexural Modulus 2.28 GPa330 ksi
Compressive Strength 82.7 MPa12000 psi10% Deflection
Coefficient of Friction 0.140.14Dry vs.Steel
Limiting Pressure Velocity 0.560 MPa-m/sec16000 psi-ft/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°F
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air 240 °C464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW037 / 296603

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.