MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema OREVAC® 18732P Grafted Maleic Anhydride Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P are mainly used in application where mechanical and adhesive performances at high temperatures are required. These Orevac are used as tie layer in 3 layer polypropylene coatings (epoxy primer / adhesive / polypropylene) for external protection of steel pipe.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Particle Size <= 125 µm<= 125 µm20%
 100 - 300 µm100 - 300 µm65%
 300 - 400 µm300 - 400 µm15%
 >= 400 µm>= 400 µm0%
Melt Index of Compound 6.0 - 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 - 10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6.06.0ISO 608
Tensile Strength at Break 20.0 MPa2900 psiISO R 527-2
Elongation at Break 500 %500 %ISO R 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FDSC
Vicat Softening Point 120 °C
@Load 0.999 kg
248 °F
@Load 2.20 lb
ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 18707 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18729 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18732 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18722 Maleic Anhydride Modified Polypropylene
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel

PARKG161 / 80122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.