MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Honeywell Aclon™ 1090 Resin  (discontinued **)
Categories: Polymer; Film

Material Notes: Superior barrier protection for containers
  • Ideal material for multilayer containers with core or contact layers
  • Clear resin with high moisture and chemical barrier
  • Plasticizer and stabilizer-free
  • Biochemically inert
  • Information provided by Honeywell

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 2.144 g/ccISO 1183
    Bulk Density 1.16 g/ccISO 60
    Water Vapor Transmission 0.248 g/m²/day
    @Temperature 37.8 °C
    100%RH; ASTM F1249
    Thickness 25.0 microns
    Melt Flow 8.0 g/10 minISO 1133
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 26.0 MPaISO 527
    Tensile Strength, Yield 43.0 MPaISO 527
    Elongation at Break 16 %ISO 527
    Elongation at Yield 7.0 %ISO 527
    Flexural Strength 61.0 MPaISO 178
    Flexural Modulus 1.604 GPaISO 178
    Izod Impact, Notched (ISO) 3.20 kJ/m²ISO 180
    Izod Impact, Unnotched (ISO) 74.0 kJ/m²ISO 180
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 214 °CCrystalline, initial; DSC
     216 °CCrystalline, remelt; DSC
    Deflection Temperature at 0.46 MPa (66 psi) 104 °CISO 75
    Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75
     
    Optical PropertiesOriginal ValueComments
    Haze 1.0 %
    @Thickness 0.0250 mm
    Film; ASTM D1003
     
    Descriptive Properties
    Zero Strength Time80-90 secondsASTM D1430

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Ensinger Delrin® 150 Homopolymer Acetal (POM)
    Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
    Beijing Evergrow Resources PTFE Porous Film
    Fiberglass Grade B
    Goodfellow CVD Graphene Film on Copper Foil

    PAL9109 / 23091

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.