MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lotte Advanced Materials Starex® TH-1100 PC, Unreinforced FR  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 17 g/10 min
@Load 10.0 kg,
Temperature 250 °C
17 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.7 MPa9250 psi5 mm/min; ASTM D638
Flexural Strength 94.1 MPa13600 psi2.8 mm/min; ASTM D790
Flexural Modulus 2.16 GPa313 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched >= 0.490 J/cm
@Thickness 3.17 mm
>= 0.918 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
@Thickness 6.40 mm
266 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 144 °C291 °FB/50; ISO R306
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %
@Thickness 3.20 mm
2.0 %
@Thickness 0.126 in
ASTM D1003
Transmission, Visible 86 %
@Thickness 3.20 mm
86 %
@Thickness 0.126 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® FD-1102 PC, FR
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Lotte Advanced Materials Infino® EN-1052 PC, FR
Lotte Advanced Materials Infino® FD-1122 PC, FR
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade

PSAMSU904 / 146721

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.