MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PSM Industries Pacific Sintered Metals FX-226-T Infiltrated Iron Powdered Metal (MPIF FX-1000-25)
Categories: Metal; Ferrous Metal

Material Notes: Machines and plates well. Good in hydraulic applications. Moderate tolerance control.

Equivalent MPIF Specification: FX-1000-25

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.20 - 7.50 g/cc0.260 - 0.271 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6565
Tensile Strength, Ultimate 352 MPa51000 psi
Tensile Strength, Yield 221 MPa32000 psi
Elongation at Break 7.0 %7.0 %
Modulus of Elasticity 110 GPa16000 ksi
Flexural Strength 910 MPa132000 psiTransverse Rupture
Charpy Impact, Unnotched 33.9 J25.0 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries Pacific Sintered Metals F-200-P Iron Powdered Metal (MPIF F-0000-10)
PSM Industries Pacific Sintered Metals FC-208-N Copper Iron Powdered Metal (MPIF FC-2000-K-40)
PSM Industries Pacific Sintered Metals FC-203-N Copper Iron Powdered Metal (MPIF FC-1000-20)
PSM Industries Pacific Sintered Metals FN-251-S Invar Powdered Metal
PSM Industries Pacific Sintered Metals FN-250-S Nickel Iron Powdered Metal (MPIF FN-0200-20)

NPACIF025 / 86183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.