MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huber Hubercarb® W3N Calcium Carbonate Powder
Categories: Ceramic

Material Notes: Hubercarb® W Series calcium carbonate has a purity level of 99.3% and is mined from a limestone deposit and processed in Quincy, IL, USA. The W Series products are ideal for applications that require high-filler loadings, low moisture content and silica content below detectable levels. In addition to being low in silica, these products are also low in trace metals like iron. Low iron content reduces undesirable degradation in some polymer systems.

Information provided by Huber Engineered Materials.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.70 g/cc2.70 g/ccASTM D-153
Bulk Density 0.801 g/cc0.0289 lb/in³Compacted; ASTM C-110
 0.881 g/cc0.0318 lb/in³Loose; ASTM C-110
Brightness 92 %92 %Dry, Hunter Reflectance
Oil Absorption 15 %15 %ASTM D-281
Solubility in Water 0.0035 %
@Temperature 100 °C
0.0035 %
@Temperature 212 °F
Moisture Absorption 0.200 %0.200 %ASTM D-280
Particle Size 2.8 µm2.8 µmMedian, SediGraph
Particle Mesh Size 325 Mesh325 MeshResidue < 0.005%
pH 9.49.4saturated solution; ASTM D-1208
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 3.03.0relatively non-abrasive
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 µm/m-°C2.39 µin/in-°F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.601.60
 
Descriptive Properties
Alkalinity0.4 mg/gmas NaOH, ASTM D-1208
ColorWhite
Composition, Calcium Carbonate (%)99.3
Composition, Iron (ppm)40
Composition, Leachable Chlorides (ppm)< 5
Composition, Magnesium Carbonate (%)0.4
Composition, Other (%)0.23
Composition, Silicas and Silicates (%)0.05
Hegman Grind6ASTM D-1210
Particle ShapeIrregular, uniaxial

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER991 / 293345

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.