MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Celanese Coolpoly® D3606 Thermally Conductive Polyamide 4,6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.

CoolPoly D3606 is a thermally conductive injection molding resin based on a Polyamide 4,6 (PA 4,6) matrix. CoolPoly D3606 is electrically insulative. Thermally conductive polymers like CoolPoly D3606 cool faster than standard injection molding grade resins.

Information provided by Cool Polymers, Inc.

D3606 has been replaced by D3608

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Water Absorption 1.2 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D551
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 90.0 MPaISO 527-1
Elongation at Break 1.0 %ISO 527-1
Tensile Modulus 12.0 GPaISO 527-1
Flexural Strength 150 MPaISO 178
Flexural Modulus 11.0 GPaISO 178
Charpy Impact Unnotched 2.00 J/cm²ISO 179-1
Charpy Impact, Notched 0.450 J/cm²ISO 179-1
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.50 J/g-°CASTM E1461
Thermal Conductivity 1.50 W/m-KASTM E1461
Flammability, UL94 V-0
@Thickness 1.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 290 - 310 °C
Middle Barrel Temperature 300 - 315 °C
Front Barrel Temperature 305 - 320 °C
Nozzle Temperature 310 - 330 °C
Melt Temperature 310 - 316 °C
Mold Temperature 80.0 - 150 °C
Drying Temperature 104 °C
Dry Time 12 hour
Moisture Content 0.050 %
Dew Point -40.0 °C
Injection Pressure 70.0 - 105 MPa
Hold Pressure 35.0 - 70.0 MPa
Back Pressure 0.000 - 0.700 MPa
Screw Speed 50 - 150 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Coolpoly® D1202 Thermally Conductive Polypropylene
Celanese CoolPoly® D3608 Thermally Conductive High Temperature Polyamide (HTN)
Celanese CoolPoly® E1201 Thermally Conductive Polypropylene
Celanese CoolPoly® E8101 Thermally Conductive Thermoplastic Elastomer
Celanese Coolpoly® D4302 Thermally Conductive Polybutylene Terephthalate

PCOOL06 / 29007

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.