MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Description: Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grade exhibits good high-temperature load-bearing capabilities. It is especially used for thinner walled and longer flow length parts requiring low flash behavior. Good weldability due to a modest filler level. Commonly used in electrical connectors and other thin wall/long flow length parts.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Water Absorption at Saturation 0.020 %ISO 62
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100ISO 2039-2
Tensile Strength at Break 150 MPa5 mm/min; ISO 527-2/1A
Elongation at Break 1.2 %5 mm/min; ISO 527-2/1A
Tensile Modulus 15.7 GPa1 mm/min; ISO 527-2/1A
Flexural Strength 230 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact Unnotched 2.80 J/cm²ISO 179/1eU
 2.80 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 4.7
@Frequency 10000 Hz
IEC 60250
Dielectric Strength 25.0 kV/mmIEC 60243-1
Dissipation Factor 0.0080
@Frequency 10000 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 41.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
Melting Point 280 °CISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 215 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
Oxygen Index 47 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 585 - 635 °F
Middle Barrel Temperature 590 - 640 °F
Front Barrel Temperature 600 - 640 °F
Nozzle Temperature 600 - 640 °F
Melt Temperature 310 - 340 °C
Mold Temperature 135 - 160 °C
Drying Temperature 275 °F
Dry Time 3 - 4 hour
Injection Pressure 5000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Celanese Fortron® 1140 L6 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese Fortron® 1140 L7 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese FORTRON ICE 716A PPS, 65% Mineral / Glass Reinforced

PHCW49 / 45990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.