MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Pocan® T 7141 000000 PET+PBT, 40% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PET+PBT 45% glass fibers, improved flowability

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Filler Content 40 %40 %Glass Fiber
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inPlaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inPlaque 60 x 60 x 2mm; ISO 294-4
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 280 °C
25 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ISO 527-1,-2
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527-1,-2
Tensile Modulus 12.0 GPa1740 ksi1 mm/min; ISO 527-1,-2
Flexural Strain at Yield 2.0 %2.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 260 °C500 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FMethod Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FMethod Bf; ISO 75-1,-2
Glow Wire Flammability Index 750 °C
@Thickness 0.800 - 3.00 mm
1380 °F
@Thickness 0.0315 - 0.118 in
IEC 60695-2-12
Shrinkage, MD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Flow Direction Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Shrinkage, TD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FPlaque 60 x 60 x 2mm
Mold Temperature 80.0 °C176 °FPlaque 60 x 60 x 2mm
Hold Pressure 60.0 MPa8700 psiPlaque 60 x 60 x 2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
BLUESTAR PBT 6630 30% Glass Filled
BLUESTAR PBT 403M-G20 20% Glass Filled
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry)
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT

PLANW9040 / 208464

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.