MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
APCM DA 4080/4082 Epoxy Pregpreg System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DA 4080 and DA 4082 are 200°F cure modified epoxy prepreg systems which can be pre-preged on fiberglass fabric, woven Kevlar, or other woven fabrics. In addition to their low temperature cure capabilities, DA 4080 prepregs have excellent flow to allow for vacuum bag cure conditions. DA 4080 is a one sided pre-impregnated system yielding a single sided tack material. DA 4082 is the same system except that both sides of the fabric are coated yielding a double sided tack material. Both prepregs can be used for laminating and honeycomb sandwich construction.

Mechanical Properties: Based upon a 0.125 inch thick cured laminate of DA 4080 prepreg containing 7781 glass at a 38% resin content. Laminates were cured at 200°F (93.3°C) for one hour at 20 psi.

Information provided by Adhesive Prepegs for Composite Manufacturers, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 50000 psi
Tensile Modulus 3.20e+6 psi
Flexural Strength 75000 psi
Flexural Modulus 3.20e+6 psi
Compressive Strength 55000 psi
Shear Strength 9000 psiShort Beam
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Pressure 0.138 MPa,
Temperature 93.3 °C
Shelf Life 0.660 Month
@Temperature 23.9 °C
 6.00 Month
@Temperature 4.44 °C
 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
CarrierAny commercial woven fabric
ColorOff White
FormModerate tack resin on woven fabric
SeparatorRelease paper and poly film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
APCM DA 4090/4092 Epoxy Pregpreg System
APCM DA 4518U/E-Glass Unidirectional E-Glass Epoxy Prepreg
Carbon-Core 10 mm+18 oz WR both sides Composite Panels

PAPCM001 / 187014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.