MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Matexcel CER-0064 Mica commutators
Categories: Ceramic

Material Notes: COMMUTATOR M & P sheets are hard, dense mica plates used in segments, separators and spacers. They exhibit good electrical & thermal properties and mechanical strength. COMMUTATOR M & P sheets can be sawed, sheared and punched into customized shapes. Its superior uniformity enables automatic feeding and stacking within high speed assembly operations. COMMUTATOR M & P sheets are used within a wide range of small and medium size commutators for all kind of household applications, industrial equipment and power tools.

Mica commutators

Key Words: Synonyms: Mica commutators
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 200 - 2000 µm200 - 2000 µm
 
Descriptive Properties
ComponentsCOMMUTATOR M & P sheets consist of minimum 90% Muscovite alternatively Phlogopite impregnated with a specially developed epoxy resin.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1501 / 300132

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.