Dry as molded. Nylene NX3024F is a medium viscosity nylon 6 resin suitable for general purpose molding applications. In addition to excellent melt stability and good melt strength, NX3024F has
excellent grease resistance, toughness, resistance to abrasion, and does not absorb food
odors. Nylene NX3024F meets the requirements of FDA regulation 21 CFR 177.1500 for
direct food contact. Optimum processing conditions should provide a melt temperature of 480
- 500ºF at the die. Data provided by the manufacturer |