MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hybrid Plastics POSS® MA0702 MethacrylIsobutyl-POSS®
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Siloxane; Thermoset; Methacrylate

Material Notes: POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS® molecules are physically large ranging from approximately 1-3 nm. POSS® materials are thermally and chemically more robust than silicones and their nanostructured architecture imparts unique properties by controlling polymer chain motion at the molecular level.

POSS®-Methacrylates possess a hybrid inorganic-organic three-dimensional structure, which contains from one to eight methacryl groups. The majority of POSS®-Methacrylates contain seven non-reactive organic groups and one methacryl group. While the monofunctional methacrylates can be incorporated into thermoplastics by copolymerization or grafting, the multifunctional methacrylates can be used as effective cross-linkers.

They react similarly in polymerization, grafting and cross-linking reactions to standard organic monomers. While reacting similarly to simple organic methacrylates, POSS®-Methacrylates impart significant improvements in the thermal, mechanical, and gas separation properties of traditional plastics.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 943.64 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 114 °C
Decomposition Temperature 290 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Budd DSM-949, Diesel Grade SMC, Vinyl Ester, Black
Multibase Dow Corning® 4-7081 Siloxane Powder Resin Modifier
Hybrid Plastics POSS® MA0750 TrisMethacrylIsobutyl-POSS®
Dow XIAMETER® PMCPPMX-0344 Cyclosiloxane Blend
Dow 230 Fluid

PHYBR002 / 78812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.