MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Assab Steels 7210M Machinery Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: ASSAB 7210M is an alloyed case hardening steel with high core strength.

Applications: ASSAB 7210M is used for applications requiring a hard, wear resistant surface and a tough core, such as transmission components for the automotive industry.

ASSAB 7210M is used for complicated parts, subject to strict demands on dimensional stability, core hardness and toughness.

AISI /SAE 3115, DIN 15CrNi6, BS 637A16 (EN 352), AFNOR 16Nc6, JIS SNC21, SS 2511

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217maximum hot rolled supplied
 200 - 35063 mm diameter. Core strength in hardened condition.
 300 - 405
@Diameter 11.0 mm
Core strength in hardened condition,
Hardness, Rockwell C <= 2530 mm from the quenched end.
 21 - 3510 mm from the quenched end.
 55tempering temperature 300°C.
 64tempering temperature 100°C.
Tensile Strength, Ultimate 690 - 980 MPa
@Diameter 63.0 mm
Rm. Core strength in hardened condition.
 980 - 1320 MPa
@Diameter 11.0 mm
Rm. Core strength in hardened condition.
Tensile Strength, Yield >= 440 MPa
@Diameter 63.0 mm
Re. Core strength in hardened condition.
 >= 640 MPa
@Diameter 11.0 mm
Re. Core strength in hardened condition.
Elongation at Break >= 11 %63 mm diameter. Core strength in hardened condition.
 >= 8.0 %
@Diameter 11.0 mm
Core strength in hardened condition,
Reduction of Area >= 30 %63 mm diameter, Core strength in hardened condition,
 >= 30 %
@Diameter 11.0 mm
Core strength in hardened condition,
Impact Test 30.0 J63 mm diameter. Core strength in hardened condition.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.15 %
Chromium, Cr 0.80 %
Iron, Fe 96.6 %
Manganese, Mn 0.90 %
Molybdenum, Mo 1.2 %
Nickel, Ni 0.10 %
Silicon, Si 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
AISI 4340 Steel, normalized, 25 mm round
AISI 4150 Steel, oil quenched 830°C (1525°F), 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 8620 Steel, annealed 13 mm (0.5 in.) round
AISI 1018 Steel, cold drawn

NASSAB20 / 15038

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.