MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: PC+ABS; Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Linear Mold Shrinkage 0.004 - 0.007 cm/cmASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 50 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 89.0 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.57 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 5.34 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
UL File E155285
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 510 °F
Middle Barrel Temperature 475 - 525 °F
Front Barrel Temperature 475 - 550 °F
Nozzle Temperature 475 - 550 °F
Melt Temperature 475 - 550 °F
Mold Temperature 135 - 185 °F
Drying Temperature 205 °F
Dry Time 2 - 4 hour
Injection Pressure 10000 - 16000 psi
Back Pressure 25.0 - 100 psi
Screw Speed 25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR3010 HF PC/ABS Blend
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy

PZ9PU42q / 140954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.