MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydrol® UH 340/1 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aliphatic anionic polyurethane dispersion. As a binder in the formulation of highly flexible water-thinnable coatings for wood, metal, plastics and mineral substrates. Also as a combination binder to improve the elasticity and flexibility of water-thinnable coatings.

Properties / Applications: Bayhydrol® UH 340/1 can be used as the sole binder in the formulation of flexible lightfast coatings. The product is also suitable for combination with other water-thinnable binders. The pH of ready-to-use coatings should be between 7 and 8. Substances such as ammonia can be used to adjust the pH. Yellowing has sometimes been observed on maple. A test area should be coated before application on large surfaces.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccDIN EN ISO 2811-2
Volatiles 59 - 61 %59 - 61 %1g/1h/125°C; DIN EN ISO 3251
Particle Size 120 - 220 µm120 - 220 µm
pH 6.0 - 7.06.0 - 7.0DIN ISO 976
 
Chemical PropertiesMetricEnglishComments
Acid Value 1.51.5[mg KOH/g]; DIN EN ISO 2114
 
Descriptive Properties
Appearancemilky, cloudy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0172 / 201955

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.