MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt AL 719 Aluminum Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Solder/Braze Alloy

Material Notes:

Applications:AL 719 filler metal is generally used to join aluminum and aluminum alloys. It has been used to join castings and otherwise unbrazeable aluminums. Care must be taken to be sure that the heat treatment (if any) is compatible with the brazing materials and process. Because of this high alloy content of AL 719, the corrosion resistance is not as good as other aluminum filler metals.

Characteristics:AL 719 is a filler metal for use with brazeable aluminums where a flux process is used. Because of its high zinc content this material is not recommended for vacuum brazing. To prevent liquation, it is recommended that the parts be heated rapidly thru the solidus-liquidus temperature range.

Specifications: AL 719 meets the requirements for the following specifications-Aluminum Association (AA) 4245

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.91 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 960 - 1040 °F
Solidus 960 °FMelting Point
Liquidus 1040 °FFlow Point
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1020 - 1060 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 72.74 %
Chromium, Cr <= 0.070 %
Copper, Cu 3.3 - 4.7 %
Iron, Fe <= 0.80 %
Magnesium, Mg <= 0.070 %
Manganese, Mn <= 0.070 %
Other, each <= 0.050 %
Other, total 0.15 %
Silicon, Si 9.3 - 10.7 %
Zinc, Zn 9.3 - 10.7 %
 
Descriptive Properties
ColorGrayish-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey LM™ 210 Indium Bearing Soft Solder Alloy
AMG Aluminum Tibor® 1.7% Ti - 1.4% B Titanium Boron Aluminum Alloy
AMG Aluminum Boral® 10% Boron Aluminum Alloy
AMG Aluminum 8% Lead Aluminum Alloy
AMG Aluminum 3% Zirconium 2% Vanadium Aluminum Alloy

NLUCMI02 / 18069

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.