MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ELASTO UK Mediprene™ 500750M TPE, Medical Applications, 75A Hardness
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:
  • Low extractable
  • No migration of plasticizer
  • Cleanliness
  • Good vapor and gas transmission properties
  • Softness, flexibility and clarity
  • Chemical inertness
  • Ease of sterilization for repeated use

Mediprene™ compounds can be processed using conventional thermoplastic equipment for extrusion, injection molding, etc. The compounds are not hygroscopic, and thus do not need any pre-drying. Assembling Mediprene™ to mainly all used thermoplastics is feasible.

All Mediprene™ grades are fully recyclable and where possible reprocessable during manufacturing and when burned do not emit toxic fumes.

Mediprene™ grades exhibit excellent resistance to many fluids used in the healthcare environment.

Information from Vita Thermoplastic Polymers (VTP).

Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
@Thickness 4.00 mm
ASTM D2240
Tensile Strength at Break 18.0 MPaASTM D638
Elongation at Break 700 %ASTM D638
100% Modulus 0.00300 GPa
@Strain 100 %
ASTM D638
300% Modulus 0.00450 GPa
@Strain 300 %
ASTM D638
Tear Strength 36.0 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 210 °C
 
Descriptive Properties
Chemical ResistanceGoodExcluding organic solvents, aromatic and vegetable oils
ColorTranslucent
Weather ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELASTO UK Mediprene™ 500520M TPE, Medical Applications, 52A Hardness
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness
ELASTO UK Mediprene™ 500600M TPE, Medical Applications, 60A Hardness
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding
ELASTO UK Mediprene™ 500900M TPE, Medical Applications, 90A Hardness

PVTC135 / 72204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.