MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huntsman IROGRAN® PS 455-215 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878ASTM D2240
Hardness, Shore D 3131ASTM D2240
Tensile Strength at Break 39.2 MPa5690 psiASTM D412
Elongation at Break 610 %610 %ASTM D412
50% Modulus 0.689 MPa
@Strain 50 %
0.689 MPa
@Strain 50 %
ASTM D412
100% Modulus 1.24 MPa
@Strain 100 %
180 psi
@Strain 100 %
ASTM D412
300% Modulus 5.52 MPa
@Strain 300 %
800 psi
@Strain 300 %
ASTM D412
Rebound 45 %45 %Bayshore; ASTM D2632
Tear Strength 57.8 kN/m330 pliASTM D624
Taber Abrasion, mg/1000 Cycles 1010ASTM D3389
Abrasion 5454mm3; DIN 53516
Compression Set  34 %
@Temperature 22.8 °C,
Time 79200 sec
34 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 82 %
@Temperature 70.0 °C,
Time 79200 sec
82 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 - 142 °C264 - 288 °FTMA Melt Range
Vicat Softening Point 61.0 °C142 °FASTM D1525
Glass Transition Temp, Tg -32.0 °C-25.6 °FMidpoint; ASTM E 1269

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® PS 455-204 TPU-Polyester
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Huntsman IROGRAN® PS 443-201 TPU-Polyester
Huntsman IROGRAN® PS 440-200 TPU-Polyester
Huntsman IROGRAN® PS 370-202 TPU-Polyester

PHUQ113 / 159486

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.